Concrete floor preparation for epoxy in Kansas City means three things done in order: getting contamination out of the slab, opening the surface to a measured roughness, and repairing cracks and joints, because a resin floor bonds only as well as the concrete under it. Moisture is checked alongside, and the coating manufacturer's written instructions set the target for each step.
Why preparation decides whether a coating stays down
A federal guide specification for chemical resistant floors puts it in one line: "Proper preparation of substrate is essential for satisfactory performance of resinous floor systems" (UFGS 09 67 23.14).
The ASTM practice for preparing concrete by abrasion explains what preparation is for. It is "intended to create a surface profile in concrete and to remove foreign materials and weak surface laitance" (ASTM D4259). Surface profile means how rough the prepared concrete is. Laitance is the weak, dusty skin that forms on top of a slab as it is finished. A coating stuck to laitance is only as strong as that skin.
The federal thin film flooring specification names three causes of early coating failure it wants a condition assessment to catch: low surface strength, heavy surface contamination such as oils, fuels, fats and waxes, and a high rate of moisture vapor emission from the slab (UFGS 09 67 23.15). Preparation deals with the first two directly. The third is a testing question.
Start with a condition check of the slab
Before anyone picks a method, someone has to look at the floor. The chemical resistant specification says existing floors "should be carefully inspected to determine condition", and the thin film specification calls a concrete condition assessment "highly recommended" before installation.
A useful condition check answers these questions:
- Is the surface concrete sound, or dusty and weak?
- Where are the oil, grease and fluid stains, and how deep do they go?
- Is there an old coating, paint, sealer or curing compound on the slab?
- Is there tile or another floor covering to come up first?
- How many cracks, joints and spalls are there, and are any slab edges curled?
- What does a moisture test say? See our guide to concrete moisture testing before epoxy.
Degreasing comes before any grinding or blasting
Oil in concrete is dealt with before the surface is opened up, not after. The federal thin film specification degreases first, on coated and uncoated concrete alike, and rinses until "the rinse water appears clear" (UFGS 09 67 23.15).
The same specification gives a simple spot check anyone can understand. Put a few drops of water on a suspect area. If the water soaks in, the surface is free of oil. If the drops "bead up and do not flatten out", the spot needs more degreasing.
The method follows the contamination. The chemical resistant specification matches them in a table: oil, fat or wax calls for mechanical or steam cleaning; paint calls for mechanical cleaning or stripping; adhesive, dust, form oil, sealers and curing compounds call for mechanical cleaning (UFGS 09 67 23.14).
Surface profile: how rough the concrete should be
Resin coatings need something to grip. The Concrete Surface Profile scale, known as CSP, is a reference developed by the International Concrete Repair Institute "to help ensure a standard for surface profiles for coatings and toppings" (CSP Profile Comparison). The required profile depends on the system being installed, and the prepared floor is checked by comparing it with a set of reference chips.
The federal thin film specification gives a worked example for its own system. It shot blasts the whole floor to CSP 3, prepares edges and spots the blaster cannot reach by diamond grinding to CSP 2 or light scarifying to CSP 4, and sets an upper limit of CSP 5 for the surface it will coat (UFGS 09 67 23.15). It also notes that primer thickness follows the profile: a rougher surface takes a thicker primer. A troweled topping or a different coating may call for another target, so the manufacturer's data sheet sets the number.
Shot blasting, grinding, scarifying and acid etching compared
| Method | What it does | Where the sources place it |
|---|---|---|
| Shot blasting | Steel shot thrown at the slab and recovered, roughening the surface and removing laitance | The federal thin film specification uses it on the whole floor to reach CSP 3 |
| Diamond grinding | Rotating diamond tooling abrades the surface | The same specification uses it at edges and spots a blaster cannot reach, to CSP 2 |
| Scarifying | Rotating cutters chip into the surface | Used for light profiling to CSP 4 and to level curled slab ends at joints in the same specification |
| Acid etching | An acid solution reacts with the surface, followed by a thorough rinse | A recognized ASTM practice to alter the profile and remove laitance (ASTM D4260), followed by a pH check of the rinsed surface (ASTM D4262) |
| Other mechanical cleaning | Stripping and abrading to take off paint, adhesives, sealers and curing compounds | The federal chemical resistant specification's table of cleaning by contamination |
Acid etching needs its rinse checked because, in the words of the ASTM pH method, chemicals left behind "may adversely affect the performance and adhesion of coatings". The coating manufacturer's instructions and the condition of the slab decide the method. A quote should name the method and the target profile, not just "prep floor".
Removing an old coating, sealer or curing compound
A new coating cannot bond through something that is not bonded itself. The federal standard resinous flooring specification calls for the concrete to be "free of all paint, sealers, curing agents, oil, grease, moisture, dirt or any other contaminants" (UFGS 09 67 23.13).
Old coatings are harder to remove than many owners expect. The thin film specification lists shot blasting, chipping, scraping, sanding, scarifying, high pressure water and hand tools as removal methods, and warns that "in general, a coating system cannot be completely removed by shot blasting" alone. Where tile comes up first, that specification has the tile and mastic tested for asbestos before removal. If the existing coating is still sound, our page on epoxy floor repair and recoating explains when it can stay.
Cracks, joints, spalls and low spots
Repairs come after profiling and before the primer. The chemical resistant federal specification has cracks, joints and spalls filled with a material compatible with the floor surfacing before it goes down. The standard resinous flooring specification fills cracks with a compatible jointing compound, patches loose concrete as the flooring maker recommends, and keeps the slab's control and expansion joints open. The thin film specification adds detail: hairline cracks up to 1/8 inch wide are typically not repaired, wider ones can be chased and sealed, joints are cleaned out, fitted with backer rod and sealed, and the sealant cures before coating.
Some slabs are past patching. The chemical resistant specification says concrete that is "badly cracked, crumbling, punky, or deeply contaminated with oil or fat" should get a new concrete topping instead of a coating over it.
New concrete has its own waiting period
A new slab is full of mix water. The federal standard resinous flooring specification does not start its topping "until the concrete has cured a minimum of 28 calendar days", and the thin film specification tests new slabs about 60 days after the pour. Both are those specifications' rules for their own systems. The ready mixed concrete association's guidance says it can take "weeks to months" in favorable conditions for a slab to dry enough, and advises against curing compounds on floors that will be coated unless the coating maker says otherwise (NRMCA CIP 28). If you are pouring new concrete for a coated floor, tell the concrete contractor before the pour.
Dust control during preparation
Grinding and blasting concrete indoors makes silica dust. Concrete, sand and stone contain crystalline silica, and the fine dust from cutting or grinding them can cause silicosis (OSHA Fact Sheet). OSHA's construction silica standard lists floor grinders as a task with listed controls: water fed to the cutting surface, or the machine maker's dust collection system with a filter of 99% or greater efficiency, plus a HEPA-filtered vacuum between passes indoors. Dry sweeping and compressed air for cleaning are restricted where they could add to exposure (29 CFR 1926.1153).
The last clean matters to the coating too. The federal standard resinous flooring specification removes dust right before priming and allows compressed air only from a compressor with an oil and water trap, so the air does not spray oil back onto clean concrete.
Checks after preparation and before coating
Before the first coat goes down, an owner can reasonably expect these to be done:
- Profile: the prepared surface compared with the reference chips for the target CSP.
- Oil: water drop spot checks on areas that were stained.
- Moisture: test results in hand and within the manufacturer's written limit.
- Conditions: floor and air within the product's limits. The federal standard resinous flooring specification, for its own system, wants the floor dry and no colder than 60 degrees F when the topping starts.
- Cleanliness: dust removed right before priming.
If a coating fails later, these are the steps people go back to. Our guide on why epoxy floors peel or bubble explains each failure.
Floor preparation questions
Is acid etching enough for a commercial floor?
Sometimes, but mechanical preparation is what the federal flooring specifications lean on. Acid etching is a recognized ASTM practice, and the chemical resistant specification allows it for new or alkali-contaminated concrete, while the thin film specification calls for shot blasting. The coating manufacturer's instructions decide which is acceptable.
What does CSP 3 mean?
It is one step on the International Concrete Repair Institute's Concrete Surface Profile scale, and a federal guide specification uses it as the target for a shot blasted floor under a thin film coating. The prepared floor is compared against reference chips to confirm it.
Can epoxy go over a sealed or cured-and-sealed slab?
Not until the sealer is off. The federal resinous flooring specifications call for the concrete to be free of sealers and curing agents, and list mechanical cleaning as the way to remove them.
Will preparing the floor fill the building with dust?
It depends on the controls used. OSHA's silica standard lists dust controls for floor grinders: water fed to the cutting surface, or the maker's dust collection system with a filter of 99% or greater efficiency, plus HEPA vacuuming between passes indoors. Ask the contractor which control they will use and how the area will be closed off.
Sources
- ASTM International, D4259, Standard Practice for Preparation of Concrete (abrasion before coating), read 2026-11-28
- ASTM International, D4260, Standard Practice for Liquid and Gelled Acid Etching of Concrete, read 2026-11-28
- ASTM International, D4262, Standard Test Method for pH of Chemically Cleaned or Etched Concrete Surfaces, read 2026-11-28
- National Ready Mixed Concrete Association, CIP 28, Concrete Slab Moisture, 2017, read 2026-11-28
- Unified Facilities Guide Specifications, Section 09 67 23.13, Standard Resinous Flooring, November 2019, read 2026-11-28
- Unified Facilities Guide Specifications, Section 09 67 23.14, Chemical Resistant Resinous Flooring, August 2016 with Change 1 of August 2018, read 2026-11-28
- Unified Facilities Guide Specifications, Section 09 67 23.15, Fuel Resistive Resinous Flooring, 3-Coat System, February 2021, read 2026-11-28
- OSHA, 29 CFR 1926.1153, Respirable Crystalline Silica, read 2026-11-28
- OSHA Fact Sheet, OSHA's Respirable Crystalline Silica Standard for Construction, read 2026-11-28
- Sherwin-Williams High Performance Flooring, CSP Profile Comparison, read 2026-11-28
Send photos of your slab for a quote
Send wide photos of the floor, close photos of stains, cracks, joints and any old coating, and tell us what the floor is used for. Preparation is a large part of any floor price; see what an epoxy floor coating costs, or read about commercial and industrial floors. Get a Quote